Basic Information
Unit MF. C24H24O32S6Zr6 Unit MW. 1564.16
Coordination  Metal Zr Linkers 2-mercapto-Butanedioic acid,(CAS:70-49-5)
Pore Size <0.7nm Pore volume 0.139 (Vm)/0.508 (Vt) cm3/g
Surface Area BET Specific surface 510 m2/g,
Analog Structure    
Product Property
Appearance White Powder  
Particle Size  <100nm
Stability
1) UIO-66-MSA is stable in air, stable in aqueous and acidic conditions(stable in PH 1-10)
2)High thermal stability, thermal decomposition temperature about 200 ° C
Preservation
1) Keep sealed in dry and cool condition 
2) It is recommended to activate for 12 hours at 80 degree in vacuum.
Other Features
Fluorescence:NA
Applications
1) Gas (such as carbon dioxide) and pollutant adsorption. -SH could be used to remove heavy metal ions (e.g. Hg2+) 

Characterizations
XRD
XRD-UIO-66-MSA
BET
BET-UIO-66-MSA
SEM
SEM-UIO-66-MSA
FTIR
FTIR-UIO-66-MSA
References
1) P. Yang, Y. Shu, Q. Zhuang, Y. Li and J. Gu, Chem. Commun., 2019, 55, 12972-12975, DOI: 10.1039/C9CC06255F ; A robust MOF-based trap with high-density active alkyl thiol for the super-efficient capture of mercury